Hastelloy B2 Alloy Steel Coil
Width: 1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500mm, 3000mm, 3500mm, etc.
Length: 2000mm, 2440mm, 3000mm, 5800mm, 6000mm, etc.
Thickness: 0.3mm to 120mm
Jako wiodący dostawca i producent w Chinach, GNEE Steel dostarcza-opłacalne produkty ze stopów na bazie niklu-.
- Wyślij e-mail-:ss@gneesteel.com
- Tel:+8615824687445
Hastelloy B2 Steel Coil introduce
Hastelloy B2 Coil


Gnee Steel offers Hastelloy B2 Sheets and Coils, which are manufactured under the guidance of our experienced experts who ensure that advanced techniques and latest tools are used in the production process. In addition, Hastelloy B2 Sheets also offer excellent resistance to pitting and stress corrosion cracking. Hastelloy B2 Coils control other alloying elements such as chromium and iron and solve other issues related to machinability. Molybdenum is the main alloying component of Hastelloy B2 Sheets and Coils, which provides important corrosion resistance to reducing environments. Hastelloy B2 Perforated Coils are molybdenum-nickel alloys that have strong corrosion resistance to reducing environments such as sulfuric acid, hydrogen chloride gas, phosphoric acid and acetic acid. B2 Sheets are also available in customized sizes and shapes to our customers. Gnee Steel is one of the well-known suppliers and distributors of B2 Coils, always providing excellent services. The picture shows the largest batch of B2 Sheets and Coils known to date, which is a thin sheet lining for the exposed environment of a utility flue gas desulfurization unit. Due to its durability and corrosion resistance, B2 alloy perforated coils were selected as an alternative in FRP fans for handling radioactive and hazardous waste incineration. A practical problem of Hastelloy UNS N10665 plates being susceptible to intergranular corrosion is the heat affected zone of welds.
Hastelloy B2 Coils Specifications
| ASTM / ASME SB333 | |
| 1000 mm x 2000 mm, 1220 mm x 2440 mm, 1500 mm x 3000 mm, 2000 mm x 2000 mm, 2000 mm x 4000 mm | |
| 0.1mm to 12 mm Thk | |
| Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated) | |
Chemical Composition of Hastelloy B2 Sheets, Plates & Coils
| C | S | P | ||||||||
| B2 | 0.010 max | 1.00 max | 0.08 max | 0.03 max | 2.50 max | 50.99 min* | 14.50 – 16.50 | 4.00 – 7.00 | 15.00 – 17.00 | 0.04 max |
Mechanical properties of Hastelloy B2 Sheets, Plates & Coils
| Yield Strength (0.2%Offset) | |||||
| Hastelloy B2 | 8.89 g/cm3 | 1370 degree (2500 degree F) | Psi – 1,15,000 , MPa – 790 | Psi – 52,000 , MPa – 355 | 40 % |
Hastelloy B2 Alloy Coil

B2 Alloy Steel Coil

Question1: Are you a trading company or manufacturer?
Question2: Could you help to design the product?
Question3: Could you supply samples?
Popularne Tagi: Hastelloy B2 Alloy Steel Coil, China Hastelloy B2 Alloy Steel Coil suppliers, niezawodne stopy tytanu, Produkty stopu tytanu z odpornością na pełzanie, stop dla sprężyn, Produkty ze stopu tytanu z spawaniem, Zastosowanie stopu tytanu, Specyfikacje stopu
Para
NrNastępny
NrMoże ci się spodobać również
Wyślij zapytanie