A36 Sheets & Plates Specifications
Specifications for A36 Sheets & Plates. If any specification is not mentioned here, please use the contact button for quick quote.
| ASTM A36 / ASME SA36 | |
| 0.5-100mm | |
| 2000-12000 mm | |
| Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated) | |
| MS A36, (UNS K02600) |
A36 Sheets & Plates Chemical Composition
| C | 0.25 | 0.290 |
| – | 0.20 | |
| – | 98.0 | |
| – | 1.03 | |
| P | – | 0.040 |
| – | 0.280 | |
| S | – | 0.050 |
Mechanical Properties of A36 Sheets & Plates
| 7.85 g/cm3 | 0.284 lb/in3 | |
| 400 – 550 MPa | 58000 – 79800 psi | |
| 250 MPa | 36300 psi | |
| Elongation at Break (in 200 mm) | 20.0 % | 20.0 % |
| Elongation at Break (in 50 mm) | 23.0 % | 23.0 % |
| 200 GPa | 29000 ksi | |
| 140 GPa | 20300 ksi | |
| 0.260 | 0.260 | |
| 79.3 GPa | 11500 ksi |
A36 Sheets & Plates – Equivalent Grades
| MS A36 | |
|---|---|
| 50049 3.1 | |
| K02600 |
A36 Coils
A36 UNS K02600 Coils
A36 WERKSTOFF NR. 50049 3.1 Coils
A36 Strips
A36 UNS K02600 Strips
A36 WERKSTOFF NR. 50049 3.1 Strips
A36 Foils
A36 UNS K02600 Foils
A36 WERKSTOFF NR. 50049 3.1 Foils
A36 Shim Sheet
A36 UNS K02600 Shim Sheet
A36 WERKSTOFF NR. 50049 3.1 Shim Sheet



Popularne Tagi: astm a36 hot rolled mild steel checkered plate astm a36 / a36m a283 grc, China astm a36 hot rolled mild steel checkered plate astm a36 / a36m a283 grc suppliers, trawienie płyty ze stali nierdzewnej, Przetwarzanie powierzchni arkusza ze stali nierdzewnej, obróbka powierzchni płyty ze stali nierdzewnej, odporność na uderzenie ze stali nierdzewnej, Międzynarodowy arkusz ze stali nierdzewnej, Płyta ze stali nierdzewnej do dekoracji
Może ci się spodobać również
Wyślij zapytanie