Incoloy 800H Stainless Steel heat resistant Plate
video

Incoloy 800H Stainless Steel heat resistant Plate

Incoloy 800H Stainless Steel heat resistant Plate Standard Specifications

ASTM B424 / ASME SB424

2000 mm / 2440 mm / 2500 mm / 3000 mm / 6000 mm

1000 mm / 1219 mm / 1250 mm / 1500 mm / 2000 mm

0.3 mm to 20 mm

Complies with ASME A and NACE MR 175 standards
Wyślij zapytanie
Czatuj teraz

Jako wiodący dostawca i producent w Chinach, GNEE Steel dostarcza-opłacalne produkty ze stopów na bazie niklu-.

Wprowadzenie produktów

 

Incoloy 800H ss Steel heat resistant Plate introduce

Incoloy 800H Stainless heat resistant Plate

Incoloy 800H Stainless Steel heat resistant PlateIncoloy 800H Stainless Steel heat resistant Plate

Incoloy 800H stainless steel plate is a high-performance alloy that is widely used in industries such as chemical processing, oil and gas, and power generation. This alloy is renowned for its exceptional strength, resistance to corrosion, and high-temperature capabilities.

One of the significant advantages of Incoloy 800H stainless steel plate is its ability to resist carburization and corrosion even in high-temperature environments. This feature makes it ideal for use in challenging conditions, such as those found in industrial furnaces and chemical reactors.

Another feature that makes Incoloy 800H stainless steel plate popular is its high-strength properties. This alloy can withstand high-stress applications and maintain its structural integrity under extreme pressure.

Incoloy 800H Sheets and Plates Chemical Composition

C S
800H 0.05 – 0.10 1.50 max 1.00 max 0.015 max 0.75 max 39.50 min 30.00 – 35.00 19.00 – 23.00 0.15 – 0.60 0.15 – 0.60
Incoloy 800H Sheet, Plate Specifications
ASTM / ASME SB 409
1000 mm x 2000 mm, 1220 mm x 2440 mm, 1500 mm x 3000 mm, 2000 mm x 2000 mm, 2000 mm x 4000 mm
0.1mm to 12 mm Thk
Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated)

800H Stainless Steel heat resistant Plate

Incoloy 800H Stainless Steel heat resistant Plate

800H heat resistant Plate

Incoloy 800H Stainless Steel heat resistant Plate






Popularne Tagi: Incoloy 800H Stainless Steel heat resistant Plate, China Incoloy 800H Stainless Steel heat resistant Plate suppliers, stop do elastycznych kąpieli produkcyjnych, stop do zielonych wanny, stop do chłodzenia kąpieli, stop do energii jądrowej, stop do pleśni, stop do kareła do trawienia

Wyślij zapytanie

whatsapp

Telefon

Adres e-mail

Zapytanie